Effects of particle size on flotation performance in the separation …
For the copper, gold and lead, the maximum fitting recoveries were all obtained with the size fraction of −43 + 20 μm, and the flotation rates of the coarse size fraction (−100 + 74 μm) were all greater than those of the fine size fraction (−20 μm). The recovery of coarse size fractions can be stabilized in a relative short time, while ...